#47_Co3O4

Type: Sample

ObjectId: 29567 ExternalId: 11090

Created: 8/13/2025 3:38:05 PM by A09) Leppin Christian [christian.leppin@rub.de]

Updated: 8/13/2025 3:39:24 PM by A09) Leppin Christian [christian.leppin@rub.de]

Access: Public Sort Code (asc): 0

Description: Elab Identifier: , Preparation Procedure: The Co3O4 nanoparticle electrodes with a high catalyst loading (42.7 µg cm-2) were fabricated by drop-casting 100 µL of Co3O4 ink onto a gold-coated quartz crystal microbalance (QCM) resonator, which served as the substrate. The ink was prepared by dispersing Co3O4 nanoparticles in Milli-Q water to achieve a concentration of 0.5 mg mL⁻¹.

[no file attached]

: Co-O

Handover

No handover events found.

Associated Objects

All properties (except table)

Include all template properties
Type Name Value Comment
Int Type 0 Type of the physical sample --//required
Int Wafer ID 0 as engraved on the wafer (0 - no id) --//required & validationSchema=https://wafervalidation.matinf.pro/wafervalidation

The table

No properties for rendering in a table found