Composition

ElementAbsolutePercentage
O 89.825 %
Co 4.103 %
Ni 2.577 %
La 3.496 %

Associated Objects

No associated objects found.

Referenced Objects (Reverse Association)

  • 10669 241106-K3-1
    Sample

    La-Co-V-O hot deposition 500°C, La2O3: RF, 200W, 20W/min ramp, Ni: 70W, pulsed DC, 350kHz, 1.4µs, Co: DCXS-750, 70W, preanneal 1h

    Auto
  • 10670 241107-K3-1
    Sample

    La-Co-V-O hot deposition 500°C onn Sapphire (dsp) for band gap, La2O3: RF, 200W, 20W/min ramp, Ni: 70W, pulsed DC, 350kHz, 1.4µs, Co: DCXS-750, 70W, preanneal 1h

    Auto
  • 10671 241108-K3-1
    Sample

    La-Co-V-O hot deposition 500°C on Si/SIO2 with Pt-electrode layer (50nm Pt on 10nm Ta, 240731-K7-1), La2O3: RF, 200W, 20W/min ramp, Ni: 70W, pulsed DC, 350kHz, 1.4µs, Co: DCXS-750, 70W, preanneal 1h

    Auto

All properties (except table)

Type Name Value Comment
Int Measurement Area 75
Float x 40.51
Float y -22.47
String Phases ICSD-17668;ICSD-36256
Float R 2522.87 Resistance (Room Temperature) for Measurement Area 75
Float Bandgap 3.09599 eV
Float SDC Area 0.00505 cm²
Float SDC Current Density 0.954203 mA/cm²

The table

PhaseName Phase
Perovskite ICSD-17668
Spinel ICSD-36256