CL20250802_001_Co3O4#48_pristine_CV_5mVpsec_0p1M_KOH_05_CV_C01

Type: Raw Document

ObjectId: 29207

Created: 8/11/2025 11:30:27 PM by A09) Leppin Christian [christian.leppin@rub.de]

Access: Public Sort Code (asc): 90

Description:

Associated Objects

No associated objects found.

Referenced Objects (Reverse Association)

  • #48_Co3O4
    Sample

    Elab Identifier: , Preparation Procedure: The Co3O4 nanoparticle electrodes with a high catalyst loading (42.7 µg cm-2) were fabricated by drop-casting 100 µL of Co3O4 ink onto a gold-coated quartz crystal microbalance (QCM) resonator, which served as the substrate. The ink was prepared by dispersing Co3O4 nanoparticles in Milli-Q water to achieve a concentration of 0.5 mg mL⁻¹.