Operando Raman Spectroscopy
#48_Co3O4
Sample
Elab Identifier: , Preparation Procedure:
The Co3O4 nanoparticle electrodes with a high catalyst loading (42.7 µg cm-2) were fabricated by drop-casting 100 µL of Co3O4 ink onto a gold-coated quartz crystal microbalance (QCM) resonator, which served as the substrate. The ink was prepared by dispersing Co3O4 nanoparticles in Milli-Q water to achieve a concentration of 0.5 mg mL⁻¹.
A1g_amplitude_3mW_5s.png
comparision_3mW_5s.png
CV_comparision_3mW_5s.png
deconvolution_3mW_5s.png
Eg_amplitude_3mW_5s.png
F2g1_amplitude_3mW_5s.png
F2g2_amplitude_3mW_5s.png
F2g3_amplitude_3mW_5s.png